TECHNET Archives

June 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Paul Klasek <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 12 Jun 1998 13:43:29 +1000
Content-Type:
text/plain
Parts/Attachments:
text/plain (95 lines)
Hi Ken
You're right on both accounts :
1
The flow on gold is that much slower and less (down right sleepish)
"volatile" than HASL , that, yes , it is a fact .
Gold is very unkeen on shorts , it's the other end you have to watch -
vetability ( vacuum seal in store helps ).
(The planarity advantages have been aired here for ever , check TechNet
files .)
Bit more demanding on process set , obviously ; but rewarding .
2
Yes again, our guys on bare boards in HK do not want to hear about HASL
; considering the hot process no wonder ;
when I asked for HASL on the same conditions as NiAu ; it was DEARER ;
set well for both ;
to sum it up , generally , regardless of pitch the NiAu should cost you
less .
To give the sales guys a break it does depend on how they're set .
On the same note , how they are set that's how they will manipulate you
to their preferences .
Just watch their jewelery tendencies , some shops do plate (and charge)
touch more than is healthy for the joint ( all meanings) .
I found asian shops with their leaner approach to process indirectly
better as well from the intermetalics view (on volumes) .

Mind you , the comfort level transition is very similar from clean to no
clean ;
if and when you'll control the process you'll love it ; prior to that
you'll hate it .
No clean gold will make you think ; if you have no contacts or switch
pads you can make it easier on yourself by using AlphaLevel silver
(organic on top) ; it's as easy to handle as HASL and as precise as gold
. Costs as HASL (Asia) .
Gains are high , it may stretch you a bit (gold), not much .
Definitely worth it from my point of view .

See you
Paul Klasek
http://www.resmed.com



>----------
>From:  Ken Patel[SMTP:[log in to unmask]]
>Sent:  Friday, 12 June 1998 9:25
>To:    [log in to unmask]
>Subject:       [TN] PCB Manufacturer: Yield & cost for Nickel-Gold v/s HASL
>
>Is it true that Nickel/Gold plating has higher yield than HASL boards for
>fine-pitch boards during pcb manufacturing while same yield for non-fine
>pitch?
>
>If I want to convert my fine-pitch boards, it will cost little higher
>compared to HASL while non-fine pitch boards will cost more for Nickel/Gold
>finish. Is it true or a bunch of baloney from typical sales? He may want to
>scare me not to convert non-fine pitch boards to Nickel/gold which I want to
>know from you guys.
>
>
>re,
>ken patel
>
>______________________________________________________
>Ken Patel                       Phone:  (408) 490-6804
>1708 McCarthy Blvd.             Fax:    (408) 490-6859
>Milpitas, CA 95035              Beeper: (888) 769-1808
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
>information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>847-509-9700 ext.312
>################################################################
>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################