TECHNET Archives

May 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
"<Jason M. Smith>" <[log in to unmask]>
Date:
Thu, 7 May 1998 13:04:42 -0400
Content-Type:
text/plain; charset=us-ascii
X-To:
jseeger*remove_for_replies*@APPLIEDCAD.COM
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (57 lines)
the info that I have noticed it has fell under the MCM-C section because si
is still classified as a ceramic by most





Please respond to [log in to unmask]; Please respond to
      jseeger*remove_for_replies*[log in to unmask]

To:   [log in to unmask]
cc:    (bcc: Jason Smith)
bcc:  Jason Smith
Subject:  Re: [TN] silicon on silicon




Hello,
>
> If several silicon chips mounted on ceramic can be called MCM-C, and
> several silicon chips mounted on a laminated are called MCM-L. What
> would several silicon chips mounted on Silicon be called ? Would that
> fall under the MCM-C section or a completely different one ?
>
        I've understood this technique to be called, MCM-D (for
        Deposition).
--
      Jeff Seeger                             Applied CAD Knowledge Inc
      Chief Technical Officer                      Tyngsboro, MA  01879
      jseeger "at" appliedcad "dot" com                    978 649 9800
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2