Try the July 1997 issue of Printed Circuit Fabrication, "Periodic Pulse
Reverse; The New Wave in Acid Copper Plating".
Rob Schetty
LeaRonal Inc.
----------
From: TechNet Mail Forum on behalf of Tomer_2
Sent: Monday, September 15, 1997 1:55 PM
To: [log in to unmask]
Subject: [TECHNET] Pulse Plating System
Hi TechNet:
I am looking for any reference, information and user experience (as well
as advantages and disadvantages) on pulse plating system.
Thanks in advance
Tomer
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|