Dear SVA patro

Regarding your queswtions about rework of BGA

1. if you heat up more than 185°C the shape of the Ball will be somewhat
spherical ( tear drop ) depenting on the cooling time ( whether you leave
enough time to to the liquid solder to form a sphere). The size of the ball
is completely undetermined.
2. I wouldn't.
3. --
4. X-ray
5. Transmission X-ray: yes in skilled personel is on work
Voltage: depending on the board ( thickness of copper where the x-rays have
to go through). 60-80 kV are usually more than sufficient. If you have too
much noise use a higher filament current ( 0.05-0.075mA )

Best regards
Guenter Grossmann
Federal Institute of Technology Zuerich
Switzerland


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2