Change to Sn can affect flux used for wavesoldering.
Make product using proposed production material and process.
Perform environmental testing as on any new product.
Immersion Sn is often used in Europe as a solderable surface.
The testing is to protect against any nasty surprises.
On occasion have found interesting things growing or other failures on a
PCA due to some unanticipated factors. This would a cause a delay or
cancellation of a material change.
On Wed, May 29, 2013 at 6:48 AM, Torsten Hagge <[log in to unmask]
> wrote:
> Hi all,
>
> after design validation with NiAu our commercial group would like to
> continue a project with chem Sn plating. My question is if anybody has a
> study which confirm similar soldering results regarding solder quality,
> vibration and thermo cycle results to prevent a new design verification
> test (which cost several hundred hours...) if we change plating.
>
> Thanks and best regards,
> Torsten
>
> Best Regards
>
> KRISTRONICS GmbH
> Torsten Hagge
> team leader HW development &
> tech. projectmanager
> Gewerbegrund 5-9
> 24955 Harrislee
> Telefon +49 (0) 461 7741-624
> Telefax +49 (0) 461 7741-642
> [log in to unmask]
> www.kristronics.de
> Place of jurisdiction: Flensburg, commercial register: HRB 1433 FL
> CEO: Dipl.-Ing. oec. Thormod Ohm
> VAD-Id: DE 811182059
> Bank account: Deutsche Bank AG Flensburg, account 4216610, bank number
> 21570011
> IBAN: DE32 2157 0011 0421 6610 00, BIC: DEUT DE HH 215
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|