Hello everyone,

This is my first time on the forum so be gentle with me.

I wish to solder to a firewall hermetic connector with #24/20
solderwells that are plated with 5 microns of Gold over
both Alumel & Chromel using a 5s HMP solder, cored with
2% "No Clean" flux.

The environment they will be used in will typically see
temperatures in the region of -55 to +270 Deg C.

My questions are:

1.  Is the process feasible?

2.  Will non-removal of the Gold prior to soldering cause
     embrittlement?

Regards,

Pat Diamond
Weston Aerospace

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2