After reading the literature, it is more than cleaning you need to
worry about. Flux entrapment may be an issue, but I note that they did
not include any test data for thermal cycling, only stress testing. No
mention on cleaning under the component either. They did note that air
trapped under the part from the conformal coating up to and around the
part caused cracked solder joints from thermal expansion of the trapped
air. They also noted that they saw solder balls trapped under the part.
The pad sizes they recommend match the terminations, but there is no
mention of aperture reduction, which is certainly a very critical
parameter on this type of component to prevent solder ball formation. I
would qualify this component very carefully before I put it out into
production, including thermal cycling followed by microsections, full
X-ray for solder balls and joint shape/formation, thermal heatsinking,
etc. You will probably need to get down to a 50%-60% aperture reduction
to eliminate the solder balls that are sure to form under this part if
too much paste is used. Having an integral standoff should help.
I am not saying don't use this part, I am just saying there are
potentially many issues, so you should fully qualify the component. IRF
may have tested this part very comprehensively, but don't assume
anything.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kevin Glidden
Sent: Monday, November 03, 2008 7:39 AM
To: [log in to unmask]
Subject: [TN] Intl Rectifier Direct FET
Is anyone out there using these? While attractive from a design and
performance standpoint, it seems like it would be a cleaning nightmare
whether using water soluble or RMA.
http://www.irf.com/technical-info/appnotes/an-1035.pdf
http://www.irf.com/technical-info/appnotes/an-1050.pdf
Kevin Glidden
Manufacturing Engineer
Luminescent Systems Inc.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|