The reference you mention in 610C was not intended as an encouragement to
use unsupported solder as a method of modifying circuit operations. The
statement actually began life as something like " an path between
electrically non common conductors". In committee discussion there were
cases illustrated to the effect that it could be intentional and if it was
then there should not be a mandatary reaction by the standard definition.
Additional definition is provided in J-STD-001C in paragraph 9.2.4.2, f
"Solder bridging between joints except when path is present by design" which
is pretty much the same as 610C.
I do not currently have access to reliability test data, although the tests
have been conducted and there should be information available from one of
the TNers.
Mel Parrish
[log in to unmask]
Mullica Hill, NJ
----- Original Message -----
From: Roger Mack <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, May 15, 2000 3:13 PM
Subject: [TN] Solder Bridging
> > Does anyone know of a reference in the standards that comments on
allowing
> > solder bridges as a method of jumpering two neighboring pins of smt
> > devices?
> >
> > IPC-A-610C section 12.4.9 describes the defect as "A solder connection
> > across conductors that should not be joined."
> >
> > Does this imply its ok if you wanted them joined? Are there any
> > reliability concerns with doing this instead of running wire?
> >
> >
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|