Steve Collins wrote:
>
> I have a design that lends itself to being V-Grooved but I seem to recall
> either in a Forum discussion of a personal discussion that this could be
> dangerous for multilayer bd.. The reason would be that it would be possible
> to fracture an internal layer with the V-Groove panel style. When I think
> about the alternative which is to rout the board it seems to me that the
> same danger is present when you break the boards away from the tabs present
> on the panel. Does anyone else have a feel for this or have experienced any
> of the things I has discussed.
>
> Steve Collins
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ##############################################################

 Steve,

   Scoring ML is O.K. and you have already received the good
  advises. Use tool to assist in separating the boards.
  We sometimes add a hole ~ 1.0 mm at the junction of the
  scores.
  However.. be very careful with you layout. some component
  like ceramic capacitors are extreeeeemely sensitive
  and tend to crack when preasure is applied even
  when boards are separated by machine.
  Try to locate them as far as possible from the score line
  and avoid placing capacitors perpendicular to score line.

   Mickey
--
   ~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
         michael weiner    Tadiran Telecommunications Ltd
           tel: 972-3-9262937      fax: 972-3-9261803
              e-mail: [log in to unmask]
            homepage  http://www.tadirantele.com/
   ~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2