I recommend that you take a look at the solder paste manufacturers
recommendations for reflow profile. In addition to your rise rate, time
above reflow and peaks you might also need to check soak time and cool down
rate. Any important items that must be checked will be found on the solder
paste data sheet.
I have no knowlede of the datapaq profiler but make sure you are glueing
your thermocouples down, not taping. Also make all thermocouples uniform
(number of twists in the wire and size of glue dot).
Sincerely,
Brian
>Hello Technet:
>
>We need to take a temperature profile for flexible circuits (Flexes). I know
>there is
>a procedure on taking temperature profiles for PCB's.
>My question is there a difference between a PCB thermal profile with a Flex
>thermal profile.
>Are there anymore important criteria to check for besides checking peak
>temperature, time above reflow and ramp rate. I would appreciate it if you
>could help provide this information.
>We are currently using Datapaq's Reflow Tracker to track our profile but
>have not provided accurate thermal profile. Do you
>know whom I can contact? I would appreciate if you could help us. I look
>forward to hearing from you.
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
>
ETS, LLC - West ETS, Inc. - East
3939 N. Freya St. PO Box 47887
Spokane, WA 99207 Plymouth, MN 55447
509-483-0900 (voice) 612-553-0051 (voice)
509-483-0331 (fax) 612-553-0246 (fax)
[log in to unmask] [log in to unmask]
Benefit from a direct relationship with the manufacturer!
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|