TECHNET Archives

October 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"P. Langeveld" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, P. Langeveld
Date:
Fri, 26 Oct 2007 17:30:46 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (97 lines)
Ioan,

Do you have a chain transport or a belt conveyor. If the connector is
too close to the chain with a high thermal mass and/or there is less
turbulance in that region, the wetting temperature may not be reached.
Did you check the delta T over the width of the oven?

Peer Langeveld
> Consultant Soft Soldering Processes
> 5502 VH 8 The Netherlands

2007/10/26, Tempea, Ioan <[log in to unmask]>:
> Thanks Peer,
>
> so it's not the plating 8-{
>
> Have to play a little bit more with the reflow, forgotten to mention the connector is SMT.
>
> Regards,
>
> Ioan
>
> -----Original Message-----
> From: P. Langeveld [mailto:[log in to unmask]]
> Sent: Friday, October 26, 2007 10:48 AM
> To: TechNet E-Mail Forum; Tempea, Ioan
> Subject: Re: [TN] Component pins plating thickness
>
>
> Ioan,
>
>  The answer is 2-fold:
>
> 1. The measured finish layers are OK. The manufacturers spec however
> are, too lean.  Already in the lead age the Ni-layer should be 0.002
> mm (80 microin), the minimum Sn thickness 0.005 mm (200 microin).
> Otherwise the risk of the Sn layer is not hermetic sealing the Ni
> layer and the latter can be oxidized. And give wetting problems, and
> even more in PTH's.
>
> 2. I presume the connector is wave soldered at say, 265 dC.
> The (matte) tin has a melting point of 231 dC. Added with the thermal
> mass of the internal metal contact lips and other internal heat sinks
> in the board, the (total) contact time on the wave(s) has to be
> increased with about 1 second.
>
> Success.
>
> Peer Langeveld
> Consultant Soft Soldering Processes
> 5502 VH 8 The Netherlands
>
> 2007/10/26, Tempea, Ioan <[log in to unmask]>:
> > Hi Technos,
> >
> > I'm having a tough connector here, hard time to get all the pins soldered.
> >
> > It is matte Sn over Ni finished, measured coating thicknesses are 250 microinch Sn over 80 microinch Ni. Are these values OK? Isn't the Ni too thin and the Sn too thick?
> >
> > The manufacturer spec is 0.001mm (40 microin) minimum Sn over 0.0013 (51 microin) minimum Ni.
> >
> > Thanks for your input,
> >
> > Ioan
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV 15.0
> > To unsubscribe, send a message to [log in to unmask] with following text in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at: http://listserv.ipc.org/archives
> > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> > -----------------------------------------------------
> >
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2