Analysis is done by the most appropriate method for what is being looked
for. Impurities will be done typically by AA, whereas quantitative
determination of known major constituents such as tin can be done
gravimetrically, [or by wet chemistry as mentioned in another post].
Differences in results between measuring sites is not unknown, they quite
often are due to sampling technique, as much as analytical process.
Mike Fenner
Indium Corporation of Europe
T: + 44 1908 580 400
F: + 44 1908 580 411
M: + 44 7810 526 317
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Barmuta, Mike
Sent: Friday, May 18, 2001 11:41 PM
To: [log in to unmask]
Subject: Re: [TN] Solder Pot Analysis
Kathy: When we analyze our solderpots we use gravimetric for the Sn and AA
for the trace elements, Pb is the remainder.
Over the years we have run multiple analysis from the same sample to cross
check ourselves and outside vendors and their analytical methods. They all
vary a little bit even back to back runs using the same methods. However I
have never seen any dramatic differences between the various techniques. In
most cases the difference in Sn content is in the +/- 0.5% range. This is
close enough and anyone trying to cut it any finer is probably not living in
the real world. I've seen bigger swings in sample to sample variation and
sampling techniques.
By the way it's Kester and Keister no matter what some people would think
:>)
Regards
Michael Barmuta
Staff Engineer
Fluke Corp
Everett WA
425-446-6076
-----Original Message-----
From: Kathy Kuhlow [mailto:[log in to unmask]]
Sent: Friday, May 18, 2001 2:31 PM
To: [log in to unmask]
Subject: [TN] Solder Pot Analysis
What is the most reliable method of solder pot analysis? I know the Keister
uses the spark analysis and Alpha uses a wet chemistry method (I think).
What are the differences and which is more reliable?
TIA
Kathy
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|