Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0wHE5k-000Bj1C; Tue, 15 Apr 97 14:40 CDT |
Encoding: |
106 TEXT |
Old-Return-Path: |
|
Date: |
Tue, 15 Apr 1997 13:50:45 -0600 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"3Bz5D.0.C-K.oczKp"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
From [log in to unmask] Tue Apr 15 14: |
49:16 1997 |
X-Mailer: |
Microsoft Exchange Server Internet Mail Connector Version 4.0.994.63 |
Message-ID: |
|
Parts/Attachments: |
|
|
>
>
>To Anyone Interested,
> We have found the described problem with our acrylic conformal coatings to
>be associated with a skin that forms on the outer surfaces the coating as the
>coating goes through it's normal curing. Any coating process which deposits a
>relatively thick (both in dimension and viscosity) coating skins over and
>inhibits the evaporation of thinners and or other volatiles from the
>underlying material. If the CCA's are then introduced into an environment of
>elevated temperature (higher than processing or initial curing temperature)
>the trapped volatiles expand and form the bubbles.
> We were never successful in thinning the coating sufficiently to eliminate
>the bubbles. If a thinner material, e.g. lower viscosity, was used then the
>edge definition from the Select Coating System was not acceptable. We did not
>consider masking the CCA's as this would defeat the labor savings of a Select
>Coat System. In general the thickness which gave us acceptable
>coating/noncoating edge definition would always bubble to some degree if
>exposed to temperature.
> We were successful in eliminating the bubbles by allowing the CCA's to air
>cure at room temperature before subjecting to elevated temperature or test.
>Most probable reason is the low room temperature outgassing pressure can't
>create visible bubbles, something about pv=nrt. Minimum cure time for the
>thickness and coating we were using was on the order of 10 days. Obviously
>this is a significant problem for Demand Flow/ JIT assembly lines or those
>concerned with WIP inventory and cycle time.
>
>Semper Fi
>Tom
>
>----------
>From: Phil Bavaro[SMTP:[log in to unmask]]
>Sent: Monday, April 14, 1997 12:36PM
>To: Paul Stolar; [log in to unmask]
>Subject: Re: Bubbles in Conformal Coating
>
>Is there any chance that the boards have moisture in them which is then
>reacting with the coating?
>
>We used to get very pretty acrylic coated CCAs by prebaking the masked,
>clean assy.
>
>Phil
>
>
>
>At 7:56 AM -0500 11/8/96, Paul Stolar wrote:
>> Sometimes the cause is the CC is too thick and does not allow the
>> gaseous products to get out. Try thinning the CC.
>>
>>
>>______________________________ Reply Separator
>>_________________________________
>>Subject: Bubbles in Conformal Coating
>>Author: [log in to unmask] at Internet
>>Date: 11/7/96 5:06 PM
>>
>>
>> I threw this question out once before but I still cannot determine the
>> source of bubbles in our conformal coating process. We are using an
>> acrylic coating and a Nordson Select Coat System. The bubbles come
>> and go from day to day.
>>
>> We have looked at viscosity, temperature, humidity, pressure,
>> z-height, contamination, micro-adjust, and a few other variables. Has
>> anyone else seen this phenomenon or do you have any insight on it?
>>
>> Any help is very much appreciated.
>>
>> Thank you.
>>
>>***************************************************************************
>>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>>***************************************************************************
>>* To unsubscribe from this list at any time, send a message to: *
>>* [log in to unmask] with <subject: unsubscribe> and no text. *
>>***************************************************************************
>>
>>
>>***************************************************************************
>>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>>***************************************************************************
>>* To unsubscribe from this list at any time, send a message to: *
>>* [log in to unmask] with <subject: unsubscribe> and no text. *
>>***************************************************************************
>
>
>Regards,
>
>
>Phillip A. Bavaro
>Senior Manufacturing Engineer
>[log in to unmask]
>(619) 658-2542
>
>
>***************************************************************************
>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>***************************************************************************
>* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
>* with <subject: subscribe/unsubscribe> and no text in the body. *
>***************************************************************************
>* If you are having a problem with the IPC TechNet forum please contact *
>* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
>***************************************************************************
>
>
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|