TECHNET Archives

July 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
"Arbour, Michel" <[log in to unmask]>
Date:
Thu, 10 Jul 2003 09:07:15 -0400
Content-Type:
text/plain
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Arbour, Michel" <[log in to unmask]>
Parts/Attachments:
text/plain (52 lines)
Thank you for your responses .
It was very informative
Regards
Michel Arbour

> -----Original Message-----
> From: Arbour, Michel [SMTP:[log in to unmask]]
> Sent: Tuesday, July 08, 2003 10:48 AM
> To:   [log in to unmask]
> Subject:      [TN] Operating temperature of PCB
>
> Hello techies,
> We have a PCB that is subjected to high temperature during normal
> operation
> of the product (Power converter).
> - There is a heat-sink mounted directly on the PCB on the top side.
> - The Dimension of the PCB is : 8" X 3". The heat-sink dim. is : 2" X 4" .
> - There is mostly copper planes in the heat-sink  area of the PCB .
> - The temperature is measured at the bottom side of the PCB and the worst
> case temperature is 110C (around 245F) .
> - It is a 6 layer PCB thickness of 0.062" .We are using a high temp FR4 .
>
> Are there any chances of degradation of the PCB over time at these
> temperature.
> Any reliability issues to adress
> Is 175C Tg sufficient .
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2