TECHNET Archives

August 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Ryan Grant <[log in to unmask]>
Date:
Wed, 30 Aug 2000 08:04:34 -0600
X-To:
"Kubes, Romeo (NM75)" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Ryan Grant <[log in to unmask]>
Parts/Attachments:
text/plain (72 lines)
Yes, what you have been told is correct.  However, I personally recommend a
0.005" thick stencil for better paste release out of such a small aperture;
especially if you have fine pitch on the same board.  Many of us are using
square apertures as well, also for better paste release and more solder
volume, without a significant increased risk of bridging.

Thanks

Ryan Grant
Advanced Technology Engineer
MCMS
(208) 898-1145
[log in to unmask]


> -----Original Message-----
> From: Kubes, Romeo (NM75) [SMTP:[log in to unmask]]
> Sent: Tuesday, August 29, 2000 4:43 PM
> To:   [log in to unmask]
> Subject:      [TN] 1 mm PBGA solder joint design requirements
>
> What are the requirements for a proper solder joint design for a 1 mm
> pitch
> PBGA.?
> (Package ball land is 0.018" dia;  ball dia is 0.026"; placed on a mixed
> technology board)
>
> I've been told to:
>
> use an equivalent 0.018" dia pad on the PWB.
>
> solder paste stencil would have 0.018" aperature dia,
>
> aperature wall will be tapered 0.001" total,
>
> Stencil thickness = 0.006"
>
> Is this industry std?
>
> R Kubes
> Honeywell
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2