TECHNET Archives

September 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Jac Kroeker <[log in to unmask]>
Date:
Wed, 15 Sep 1999 09:16:00 -0700
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Jac Kroeker <[log in to unmask]>
Parts/Attachments:
text/plain (53 lines)
Edward;
Selective solder stripping is not an easy process to do consistently well.
However in my opinion and the opinion of the customers that are prepared to
pay for the added cost it is a superior finish to HASL or HASL
alternatives. Our next best option is omikron white tin. What is your
opinion of the HASL alternatives currently available? ENIG, SILVER, WHITE
TIN, OSP.

To answer your question below.
I don't think the type of dry film photoresist is an issue. We use Dupont
9600. We found better results with a thicker emulsion than normal. 2
instead of 1.5 mil. This will help to eliminate your leaking problem.
Now you must be prepared to cheat a little.
Unless you can produce 100% perfect registration at all stages of
manufacture, you will have either bare copper at the pad edges or reflowed
solder under the mask. We do an expansion/contraction of the solder
mask/solder strip film which leaves a small annular ring of solder under
the mask. Size of the ring will depend upon your registration abilities.
Reflow the tin/lead after masking.
If you are proceeding with further testing, I will appreciate your comments.
Jac Kroeker

At 10:34 AM 09/15/1999 +0200, you wrote:
>Hi Jac,
>I am just wondering how your selective stripping is working?Probably you are
>using selective masking ( photoresist) to protect the areas destignated for
>reflow.What kind of photoresist are you using and what about overlaping
>between tin-lead stripped pattern and solder mask pattern?
>In the past we made trials and we faced the following problems:
>1) leaking of tin-lead stripping solution along lines.This resulted non
>clear boundary between the sections that were destignated for reflow and
>those destignated to be covered by solder mask.
>2) as result of the previous,we got exposed copper ar the boundary of the
>"reflow side" and tin-lead on the "solder mask" side.
>Regards
>
>Edward Szpruch
>Eltek , Manager of Process Engineering

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2