TECHNET Archives

October 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Franklin Asbell <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Franklin Asbell <[log in to unmask]>
Date:
Fri, 21 Oct 2005 17:23:46 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (52 lines)
My suggestion, and this if often made by myself and others in the public
forum...is use your supplier (solder, equipment, etc).

They want their product (chemicals, materials, equipment, etc) to work, if
there are issues they would be the best suited to help you work them
through. Their service should be free, they should be willing to do whatever
it takes and in my experience, 90% of them do...

Just one persons opinion, and of course those that oppose this opinion are
wrong...(grin)...now spend the weekend wondering if I was being truthful...

Franklin



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jason
Sent: Friday, October 21, 2005 4:46 PM
To: [log in to unmask]
Subject: [TN] Solder reflow audit

Can anyone suggest a resource offline to consult on our SMT soldering
process, We would be showing a problem and looking for solutions to remedy
the problem.

Regards,
Jason

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2