Olivia
No clean fluxes leave residues.
J-STD-001B (can't quote issue C because I don't have a copy to hand) states:
8.3.5 Flux Residues
Assemblies shall be tested in accordance with IPC-TM-650, Test Method 2.3.27
and shall comply with the following requirements for the maximum allowable
level of flux residues:
Class 1 assemblies less than 200 microgram's/sq cm
Class 2 assemblies less than 100 microgram's/sq cm
Class 3 assemblies less than 40 sq/sq cm
In case you don't know the classifications
Class 3 is safety critical products - e.g. gas meters, military hardware,
ABS, air bag or engine management stuff etc..
Class 2 is service dependant products - UPS systems, process plant control
and stuff that doesn't necessarily endanger life but matters if it breaks!
Class 1 is low consequence product - PC's, phones, toys etc..
As to the failures you mention, flux residues + moisture + electricity =
trouble.
Hope this helps.
Regards Graham Naisbitt
[log in to unmask] <mailto:[log in to unmask]>
Concoat Limited
Alasan House, Albany Park
Camberley GU16 7PH - UK
www.concoat.co.uk <http://www.concoat.co.uk>
Phone: +44 1276 691100
Fax: +44 1276 691227
Mobile: +44 79 6858 2121
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Olivia Mc Dermott
> Sent: 30 January 2002 13:48
> To: [log in to unmask]
> Subject: [TN] Flux residue with a no-clean process
>
>
> Is it OK to have flux residue on assemblies when the process is
> no clean. We
> have assemblies that are failing in the field and the customer thinks this
> flux residue may be an issue. They think the assembly has been wet.
> What do you think???? All help appreciated.
>
> _________________________________________________________________
> Join the world’s largest e-mail service with MSN Hotmail.
> http://www.hotmail.com
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources &
> Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|