Mime-Version: |
1.0 |
Content-Type: |
text/plain; charset="us-ascii" |
Old-Return-Path: |
|
Date: |
Wed, 19 Mar 1997 08:10:55 +0200 (IST) |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
X-Sender: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Loop: |
|
Resent-Message-ID: |
<"_5SjV.0.KlM.C5uBp"@ipc> |
Subject: |
|
From [log in to unmask] Thu Mar 20 10: |
44:29 1997 |
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0w7ERZ-000BBpC; Wed, 19 Mar 97 00:01 CST |
From: |
|
X-Mailer: |
Windows Eudora Light Version 1.5.2 |
Message-Id: |
|
Parts/Attachments: |
|
|
Hi Technetters !
We are in preliminary stage of design the expansion of the existing pattern
plating line ( acid copper + tin-lead ) . Most of our PCB are SMT and back
planes , up to 2.4 mm thick , 0.30 mm drilled vias , 4 - 5 mill conductors
on the outer layers . The external pattern is not equal , lot of isolated
pads and conductors . The next goal is 3.6 mm thich and 0.25 mm drilled vias
. The existing cathode - anode distance is only 4 inch . Most of the boards
are plated with current dencities in range approx. 20 ASF 60 minutes . More
complicated and with high aspect ratio : double time and half of current
dencity . Normally , we are traing to compensate uneven pattern by adding
non - functional pads on the outer layers .
Since the available space for further expansion is limited , we have to
decide which one of basic approaches should be considered :
1 ) Keep the existing cathode - anode distance , but to plate with low
current dencity ( 10 ASF ) 120 minutes .
2 ) Go to larger anode-cathode distance ( say 10 inches ) , keep the
existing plating time ( 60 minutes ) and the current dencity ( 20 ASF )
Basic points for decision :
1 ) Better surface - hole plated copper distribution in high aspect ratios
2 ) Better surface distribution to avoid overplating on isolated pads and
conductors to avoid severe overplating problems .
Your comments will be very appreciated !
Edward Szpruch
Eltek Ltd - Israel
Tel 972 3 9395050
Fax 972 3 9309581
E-mail : [log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|