I tried to use it on a recent project. We are using Merix and Sanmina
for our FAB. Both claim that they have to send it out to get that done
and the Fab that did build it used SnPb HASL and gave us a RoHS5 cert.
Failed the XRF scan, before assembly fortunately.
We disqualified RoHS HASL to avoid the problem. Just using ImAg now.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Wednesday, October 24, 2007 9:13 AM
To: [log in to unmask]
Subject: [TN] Lead-free HASL
For years we knew and loved Pb HASL. With the requirements of RoHS HASL
took a back seat. Has L-F HASL had the kinks worked out so it is
becoming a main stream process? If so, who is doing it and what is the
performance of the process? Is it being used for SMT?
Thanks in advance,
Phil Nutting
NOTICE: This e-mail transmission (and/or the attachments accompanying it) may contain confidential or proprietary information belonging to DRS Technologies or the sender. The information is only for the use of the intended recipient. If you are not the intended recipient you are hereby notified that any disclosure, copying, distribution or the taking of any action in reliance on the contents of this information is strictly prohibited. Any unauthorized interception of this transmission is illegal under the law. If you have received this transmission in error, please promptly notify the sender by reply e-mail, and then destroy all copies of the transmission.
"This (document/presentation) may contain technical data as defined in the International Traffic In Arms Regulations (ITAR) 22 CFR 120.10. Export of this material is restricted by the Arms Export Control Act (22 U.S.C. 2751 et seq.) and may not be exported to foreign persons without prior written approval from the U.S. Department of State."
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|