Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 24 Sep 2010 11:32:18 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Dharma Kemp-Bresett <[log in to unmask]>
Subject:
From:
Dharma Kemp-Bresett <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<002101cb5bfb$134a5ab0$0301a8c0@caliber>
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (237 lines)
LOL its called a contour tool, d'oh! 
Dharma

KAW/USA 
Suite 448
20 Trafalgar Square
Nashua, NH 03063
 

Confidentiality Notice: This email and any accompanying documents contain
information that is confidential, privileged or exempt from disclosure under
applicable law and is intended for the exclusive use of the addressee. This
information is private and protected by law. If you are not the intended
recipient, or have received this email in error, you are hereby notified
that any disclosure, copying, distribution or use of the contents of this
document in any manner is strictly prohibited.


-----Original Message-----
From: Dharma Kemp-Bresett [mailto:[log in to unmask]] 
Sent: Friday, September 24, 2010 11:14 AM
To: [log in to unmask]
Subject: Re: [TN] NTC: Friday quiz 18

This looks like a tool we have in our basement... I forget exactly what it
is called (and my husband is not here to answer as it is a "family heirloom"
of his) but it is a hundred or so little pins that slide in a central mount
and can be used for getting "the shape of things" like moldings and odd
contours then you can replicate them elsewhere... 
Dharma

KAW/USA
Suite 448
20 Trafalgar Square
Nashua, NH 03063
 

Confidentiality Notice: This email and any accompanying documents contain
information that is confidential, privileged or exempt from disclosure under
applicable law and is intended for the exclusive use of the addressee. This
information is private and protected by law. If you are not the intended
recipient, or have received this email in error, you are hereby notified
that any disclosure, copying, distribution or use of the contents of this
document in any manner is strictly prohibited.


-----Original Message-----
From: Inge [mailto:[log in to unmask]] 
Sent: Friday, September 24, 2010 11:05 AM
To: [log in to unmask]
Subject: Re: [TN] NTC: Friday quiz 18

Not a correct answer, Mirka.  Try harder.
/Inge


----- Original Message -----
From: "Halas, Mirka" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, September 24, 2010 3:24 PM
Subject: Re: [TN] NTC: Friday quiz 18


You are measuring the width of knitted fabric.
It is a knitting machine.
I have a fond memories of mine.

Mirka Halas
PCB Designer CID, Librarian - Eurotech North America

direct: +1 301.490.4007 x101
email: [log in to unmask]



USA - 10260 Old Columbia Road | Columbia Maryland 21046-2375 | Tel. +1 
301.490.4007 | Fax +1 301.490.4582 |
www.eurotech.com
____________________________________
This e-mail, and any file attached to it, is meant only for the intended 
recipient of the transmission and may be a communication privileged by law. 
If you have received it in error, please notify the sender immediately and 
delete the original from your system. Any other use of this e-mail by you is

strictly forbidden.
____________________________________

Please consider the environment before printing this e-mail.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Friday, September 24, 2010 9:13 AM
To: [log in to unmask]
Subject: Re: [TN] NTC: Friday quiz 18

Hi Inge,

I've was feeling pretty bad yesterday, today a little better. Got your
quizzes up for everyone to guess:

http://stevezeva.homestead.com/quiz18.jpg

http://stevezeva.homestead.com/quiz18b.jpg

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
Sent: Thursday, September 23, 2010 2:40 AM
To: [log in to unmask]
Subject: [TN] NTC: Friday quiz 18

What am I measuring? Simply  that.
And what's the hand tool for?
For some, it's peace of a cake, for others a deep mystery.
What party do you belong to?

Steve may give you a hint?

Inge

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
----------------------------------------------------- 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2