TECHNET Archives

October 2016

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Matthias Mansfeld <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Matthias Mansfeld <[log in to unmask]>
Date:
Thu, 6 Oct 2016 12:09:52 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (31 lines)
On 6 Oct 2016 at 4:59, Nigel Burtt wrote:

> Are "solvent bubbles" a peculiar problem with this type of conformal
> coating or a generic problem for coatings? 
> 
> Hypothetically if coating penetrates under the body of a low stand-off
> component and a solvent bubble remains trapped under there after the
> cure/dry, could that bubble "pop" under thermal cycling or high stress
> service environment with enough force to fracture the solder joints on
> the part?

Just a guess, but I would be afraid that the solvent (which is 
assumed to be away after curing) remains for "ever" or at least long 
enough to make trouble. Remaining solvent in any traps does, what it 
is supposeed to do: solve stuff, especially if it is well trapped in 
its own bubble and has in the worst case really long time to attack 
stuff.

Regards

Matthias

--
Matthias Mansfeld Elektronik * Printed Circuit Board Design and 
Assembly
Neithardtstr. 3, D-85540 Haar, GERMANY
Phone: +49-89-4620 0937, Fax: +49-89-4620 0938
Internet: http://www.mansfeld-elektronik.de
OpenPGP: http://www.mansfeld-elektronik.de/gnupgkey/mansfeld.asc
Fingerprint: 6563 057D E6B8 9105 1CE4 18D0 4056 1F54 8B59 40EF

ATOM RSS1 RSS2