Hi Dave,
Thanks for your input.
What exactly would happen with the IMC if the boards are baked first
before storage?
In other words: Why does the diffusion accelerate after baking? I would
presume that the acceleration of IMC growth is only temporary during the
baking process.
And , in fact, there would be no difference if the two steps are
performed in a different order.
Jowan Iven
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Wednesday, February 17, 2010 2:47 PM
To: [log in to unmask]
Subject: Re: IMC growth on ImSn
Hi Jowan! Yes, you may see a difference is the ImSn degradation
depending
on which order you conduct your baking process. The ImSn surface finish
has two degradation mechanisms - oxidation of the Sn on the ImSn surface
and diffusion of the copper into the tin creating a copper/tin
intermetallic (IMC) which has really bad solderability characteristics
once it becomes oxidized. Diffusion is a time/temperature controlled
process so if you "bake and store" the pwbs, you are effectively
assisting
the creation of the IMC, its oxidation and degrading the pwbs much
faster
than if you " store and bake". ImAg and ENIG are much more robust in
terms
of oxidation and IMC issues in comparison to ImSn but the same processes
are going to occur just on a different time scale and with different IMC
phase reactions (i.e. oxidized Ni based IMCs are not any fun to solder
either). The good news is that the many of the pwb surface finishes on
the
market today have 12 months of shelf life when stored in reasonable
temperature/humidity controlled conditions. The IPC-1601 committee is
working on a document that addresses your question.
Dave Hillman
Rockwell Collins
[log in to unmask]
"Iven, Jowan" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
02/17/2010 02:11 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Iven, Jowan" <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] IMC growth on ImSn
Hello all,
Baking boards before SMT assembly is very common.
Is there a difference between "baking and then storing the board for 6
months" and "storing the board for 6 months and then baking before
assembly" ?
Does the IMC grow faster on boards with ImSn finish after baking?
I'm especially talking about ImSn but I'm also interested in the effect
of baking on other finishes like ImAg and Enig.
Storage would be in a dry shield bag with silicagel or a dry cabinet.
Any suggestions are welcome.
Jowan Iven
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
This e-mail and any attachment is confidential and may be legally privileged or otherwise protected from disclosure. If you are not the intended recipient, please notify the sender immediately by returning this e-mail. Neways Electronics NV is not responsible for the improper or incomplete transmission of any e-mail, or for any delay in its receipt.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|