Paul, I'd say given the rotary nature of application you can really
speed up the life test quite easily with a motor and counter , just
watch the friction temp . The possible oxide consideration (build up
between cycles on nickel) is not so pronounced on rotary (or slide)
application .
Therefore you can test any surface sample you desire , the flash gold
does vary from manufacturer to manufacturer .
For that reason alone standardised specs would not supersede life test .
Give it a shoot (test) , we get good yields from NiAu on switching
(carbon pads, touch&skid)
See you paul
>----------
>From: Paul Gould[SMTP:[log in to unmask]]
>Sent: Tuesday, 24 March 1998 4:14
>To: [log in to unmask]
>Subject: [TN] FAB: Electroless Nickel/Immersion Gold for rotary contacts
>
><<File: ATT00247.html>>
>Has anyone any experience of using electroless nickle/immersion gold finish
>on rotating wiper contact areas of the pwb. Is there a spec which permits
>this. I have made circuits for wahing machines with immersion gold on copper
>and that worked with a life of about 10 years, but that was more than 20
>years ago. The problem is the cost of hard plating selected areas.
>
>Any thoughts on this would be appreciated.
>
>Paul Gould
>
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|