TECHNET Archives

December 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Joe V. Ottesen" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 15 Dec 2000 08:21:16 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (47 lines)
Julien Bouchard wrote:

> Hi everybody,
>         We recently start to use an ultrasonic stencil cleaners for our stencils.
> It' work well, but after some time, we saw a lot of fiducial that the black
> epoxy have been partially or totaly remove.  I want to know if someone had a
> similar problem with a stencil cleaner. Also, we looking for a material to
> repair the black epoxy of the fiducial ( for now we use ink pen, but we need
> to redo the job everytime we change of product). Our stencil are from UTZ
> and our stencil cleaner is from SMART-SONIC.  Thank you.
>
> Julien Bouchard
> Matrox - Process Engineer
> Email : [log in to unmask]
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------

Hi,

    I have also seen the problem, with the same cleaning equipment.
    To repair the fiducial and get the best contrast we use a Loctite 4501 kit.
    Today our stencil deliverer is pigmenting the metal in the half etched fiducial mark and
it works like a dream.


--
best regards
Joe Vella
[log in to unmask]
Website      http://www.bbelectronics.dk

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2