Julien Bouchard wrote:
> Hi everybody,
> We recently start to use an ultrasonic stencil cleaners for our stencils.
> It' work well, but after some time, we saw a lot of fiducial that the black
> epoxy have been partially or totaly remove. I want to know if someone had a
> similar problem with a stencil cleaner. Also, we looking for a material to
> repair the black epoxy of the fiducial ( for now we use ink pen, but we need
> to redo the job everytime we change of product). Our stencil are from UTZ
> and our stencil cleaner is from SMART-SONIC. Thank you.
>
> Julien Bouchard
> Matrox - Process Engineer
> Email : [log in to unmask]
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
Hi,
I have also seen the problem, with the same cleaning equipment.
To repair the fiducial and get the best contrast we use a Loctite 4501 kit.
Today our stencil deliverer is pigmenting the metal in the half etched fiducial mark and
it works like a dream.
--
best regards
Joe Vella
[log in to unmask]
Website http://www.bbelectronics.dk
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|