TECHNET Archives

December 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Date:
Tue, 30 Dec 2003 09:24:32 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, 27782 <[log in to unmask]>
Subject:
From:
In-Reply-To:
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; format=flowed; charset="iso-8859-1"
Parts/Attachments:
text/plain (47 lines)
Hi Bruce,

Sounds to me like they have an issue with maintaining their tol. thus, they
need to cover their butt. Work the issue with them, if you require mil spec
than the answer is no waiver!



Dan Mauro
Celestica Corp. (CNE)



Bruce D Stilmack writes:

> I have a PCB manufacturer requesting a waiver for the MIL SPEC requirement
> of a 2 mil annular ring.  Their position is that the coupons are from the
> edge of the laminate where the registration is worse.  The assumption is
> that the ring will be larger in the PCB itself.  I am leery to grant a
> waiver to allow this deviation, but would like to know how the community
> feels about this.
>
> Bruce Stilmack
> GDLS-TO Manufacturing Engineer
> (850) 574-4773
> [log in to unmask]
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2