TECHNET Archives

November 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Chafin, Ken G." <[log in to unmask]>
Date:
Wed, 12 Nov 2008 14:58:24 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joe Russeau <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; format=flowed; charset="iso-8859-1"; reply-type=original
From:
Joe Russeau <[log in to unmask]>
Parts/Attachments:
text/plain (134 lines)
Hi Ken,

If you are trying to look for electrochemical (ECM) failures as a result of 
the flux, then you may wish to consider doing SIR testing per IPC-TM-650, 
method 2.6.3.7.  The conditions used in this method (40 C / 93% RH with a 10 
VDC bias and test for 7 days using continuous monitoring) have been shown to 
be more stringent than using higher temperatures with high humidity (i.e. 70 
C / 95% RH), especially for low solids fluxes (i.e. no cleans).  Part of the 
drawback of using higher temperature / humidity test environments, is that 
you often cook off the very residues you are trying to observe.  Work done 
by Dr. Chris Hunt of NPL showed that lower temperatures with high humidity 
and lower biases was better for evaluating the potential for ECM events due 
to flux residues.

All that said, I would suggest evaluating the flux residues using the above 
method with a test board that is designed for SIR and has components to 
mimic modern assemblies.  The IPC-B-52 board comes to mind.

I would highly recommend that you obtain the Gerbers for the board you 
choose and have them made by your preferred supplier with your preferred 
materials and surface finish.  This may cost you a bit more, but it gives 
you an apples to apples comparison.

Secondly, it would be a good idea to compare the residues from your current 
materials against the Indium material using ion chromatography.  This will 
give you some important additional data and provide a baseline to compare to 
the SIR data and to the performance of your current paste / flux material.

Anyway, I hope this helps.

Best Regards,

Joe Russeau




----- Original Message ----- 
From: "Chafin, Ken G." <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, November 12, 2008 1:13 PM
Subject: [TN] Flux Qualification


We are trying to qualify a no-clean flux to be used in our wave solder
process.

The flux in question is Indium #9942.

After wave soldering our boards are conformal coated with polyurethane
coating Conathane CE-1164.

We have done some baking of a test sample at 70 degrees C and and have
tested per IPC-TM-650 2.6.7.1--thermal shock test.

This testing was done primarily to evaluate the adequacy of the adhesion
of the conformal coating.

We are interested in further evaluating this flux to determine if it
contributes to corrosion development or other undesirable effects.

We are considering "soaking" a sample in a chamber at 70 degrees C at
95% relative humidity for four or five days.

I am interested in any recommendations for further
testing--standards-related tests, nonstandards-related tests that may
reveal undesirable properties in the flux, etc.

Thanks



Kenneth Chafin
Quality Compliance Leader

  <file:///c:/signature/Email%20signature_files/image001.jpg>
1000 Technology Drive
Pittsburgh, PA 15219-3120
USA
Telephone: +1-412-688.2400 Ext [Ext]
Telefax: +1-412-688.2399
www.ansaldo-sts.com <http://www.ansaldo-sts.com/>



CONFIDENTIALITY
This message is strictly confidential. Its content and use is restricted
to the designated recipients. The use, copy, reproduction or transmittal
by any process or means without prior written notice of the Author or
Ansaldo STS / Union Switch & Signal Inc. office of the Legal Counsel is
strictly prohibited. If you have received this message in a transmission
error, please inform the sender immediately and destroy any copy, saved
files or print you have erroneously made.


PRIVACY:
Meeting the needs and expectations of our Customers and Employees has
always been our highest priority and that includes protecting their
privacy in compliance with local, state and federal laws and in
accordance to Ansaldo STS/Union Switch & Signal Inc. Privacy Code.


ENVIRONMENTAL NOTE:
IN SUPPORT OF OUR ENVIRONMENT, WE RECOMMEND NOT PRINTING EMAILS EXCEPT
WHEN ABSOLUTELY NECESSARY





---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2