TECHNET Archives

June 2018

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Willis Tam <[log in to unmask]>
Date:
Mon, 11 Jun 2018 11:46:19 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob Wettermann <[log in to unmask]>
Message-ID:
Subject:
From:
Bob Wettermann <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (86 lines)
Technically this is not a defect based on your description BUT you may have
to follow the golden rule-he who holds the gold makes all the rules.

The only possibility is that a form/fit/function is not satisfied due to
the existence of the scratches (would find that somewhat hard to believe
but there may be some issues if the reflection of light off of the PCB has
some impact on the circuit functioning properly).

I would suggest asking if repairs are allowed (If you can repair the mask
which is easy to do).

Also if you capitulate to their request I would make sure that the customer
spells out what the accept/reject criteria look like? How deep can the
scratches be? How long? Where?

If it's not in the spec and you are inspecting to the spec then the spec
needs to change.

Bob/BEST Inc

On Sun, Jun 10, 2018 at 8:06 PM, Willis Tam <[log in to unmask]> wrote:

> Hi All,
>
> Any comments and suggestion will be highly appreciated.
>
> B.R.
> WT
>
> -----邮件原件-----
> 发件人: TechNet [mailto:[log in to unmask]] 代表 Willis Tam
> 发送时间: 2018年6月5日 10:23
> 收件人: [log in to unmask]
> 主题: [TN] 答复: Interpretation of IPC standard for Solder Mask Scratches on
> PCBA
>
>
> Hi Technet,
>
>
> We have some arguments with one of our customers on the interpretation of
> IPC standard for Solder Mask Scratches on PCBA.
>
> According to IPC-A-610F §10.7.2. Solder Mask Coating-Voids, Blisters,
> Scratches.
> Acceptable- Class 1,2,3.
> Blister, Scratches, Voids that do not expose conductors and do not bridge
> adjacent conductors, conductor surface or create a hazardous condition
> which would allow loose mask particles to become enmeshed in moving parts
> or lodged between two electronically conductive mating surfaces.
>
>
> Customer's product specification defined the PCBA to be compliance to
> IPC-A-610F standard Glass 3.
> Customer found some scratches on solder mask surface on some of the
> PCBAs,  the scratches are minor scratches, not deep/heavy scratches, not
> expose conductors(copper traces under solder mask), but go across the
> adjacent conductors;
> We considered those scratches acceptable according to IPC-A-610F §10.7.2,
> but customer said not acceptable.
>
> The main argument is: customer considered any scratch which go across
> adjacent conductors as rejection, (Bridge adjacent conductors = go across),
> even not expose conductor.
> This is an 5mil/5mil(width/space) board, not accept scratches which go
> across adjacent conductors means not accept scratch of 10mil (0.25mm)
> length.
>
> I would like to seek clarification from IPC guru so that we move forward
>
>
> Best Regards
> Willis Tam
>
>
>
>
>


-- 
Bob Wettermann
BEST Inc
[log in to unmask]
Cell: 847-767-5745