TECHNET Archives

August 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Steven Kelly <[log in to unmask]>, "TechNet E-Mail Forum ([log in to unmask])" <[log in to unmask]>
Date:
Mon, 28 Aug 2017 16:08:04 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ed Popielarski <[log in to unmask]>
Message-ID:
Subject:
From:
Ed Popielarski <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
<52135AE4151D8343B16989B2BFBED7DA011FA19B494D@pfc-dc01>
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
Steven,



I ran across this on a custom VLSI BGA with 20+ week lead time... no choice but to "use as is" to make delivery schedule.



I put them balls up on a piece of 3mm Durastone and sprayed them generously with water soluble wave soldering flux. Ran them through the oven with 3°/sec ramp to peak, 30 sec TAL then clean in aqueous in-line system prior to placement. Worked great!



Unorthodox, butcha gotta do whatcha gotta do sometimes (said with NY accent).



Regards,



Ed Popielarski

Engineering Manager





                               970 NE 21st Ct.

                              Oak Harbor, Wa. 98277



                              Ph: 360-675-1322

                              Fx: 206-624-0695

                              Cl: 360-544-2289







       “It's one kind of victory to slay a beast, move a mountain, and cross a chasm, but it's another kind altogether to realize that the beast, the mountain, and the chasm were of your own design.”

https://goo.gl/maps/mMjg43rXeFB2





-----Original Message-----

From: Steven Kelly [mailto:[log in to unmask]] 

Sent: Monday, August 28, 2017 6:51 AM

To: Ed Popielarski

Cc: Steve Gregory

Subject: RE: [TN] Dried flux



Thanks Steve for posting these for me. 

The first picture called partial ball is a picture of one of the balls on the connector as received.

Second picture is what  the supplier has called dried flux on the connector as received Third picture shows what we call head in pillow Fourth picture - different view of third picture



Thanks for everyone's help on this . Regards Steve Kelly





-----Original Message-----

From: Ed Popielarski [mailto:[log in to unmask]]

Sent: August-25-17 2:26 PM

To: TechNet E-Mail Forum <[log in to unmask]>; Steven Kelly <[log in to unmask]>

Cc: Steve Gregory <[log in to unmask]>

Subject: RE: [TN] Dried flux



Steve Gregory (cc'ed herein) has graciously offered his time and dataspace to post Technet pix on his site.



Forward your pics to Steve, I'm certain he will oblige!

 

Regards,



Ed Popielarski

Engineering Manager





                               970 NE 21st Ct.

                              Oak Harbor, Wa. 98277



                              Ph: 360-675-1322

                              Fx: 206-624-0695

                              Cl: 360-544-2289







       “It's one kind of victory to slay a beast, move a mountain, and cross a chasm, but it's another kind altogether to realize that the beast, the mountain, and the chasm were of your own design.”

https://goo.gl/maps/mMjg43rXeFB2



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Kelly

Sent: Friday, August 25, 2017 11:13 AM

To: [log in to unmask]

Subject: Re: [TN] Dried flux



Hi all,

Want to post some pictures - can someone please give me direction. Thanks. Steve Kelly



-----Original Message-----

From: Bev Christian [mailto:[log in to unmask]]

Sent: August-25-17 11:00 AM

To: 'TechNet E-Mail Forum' <[log in to unmask]>; Steven Kelly <[log in to unmask]>

Subject: RE: [TN] Dried flux



Steve,

From what people are saying, it is more and more likely that it IS the flux residue.  You say: "On average we are getting 1-3 failures per 200 joints."  That pretty well eliminates gross part warpage.  



Minor point of interest:

With regards to part warpage (or boards), they can test fine for planarity both before and after reflow. That doesn't mean they weren't warped DURING reflow.

Bev



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Kelly

Sent: Friday, August 25, 2017 10:26 AM

To: [log in to unmask]

Subject: Re: [TN] Dried flux



Hi Dave,

The parts come vacuum sealed and after opening we have a fairly short period of time to assemble. Manufacturer also said the “dull ball” on the connector is common for lead-free solder ( agree) and is not considered related to the failure. Its’ mainly because tin constituent appears on the surface. ( I understand that) Then they say the “residue” which we identified on the ball is considered to be flux and is not related to the head in pillow.

But only a few of the 200 or so balls exhibit this issue and I am not saying we do not have other issues but we have traced some of the head in pillow to a couple of the so-called flux residue balls . On average we are getting 1-3 failures per 200 joints.

We have measured the flatness of the rigid stiffener – looks OK to us – co-planarity is .002- .004 after convection reflow.

Reviewing what Bev said yesterday- pasting – we looked at it 3 times but doing it again.

I also have pictures of what we call an incomplete ball which I would like to post but I need a refresher course on how to do this.



Thanks for everyone’s help.

Steve Kelly



From: David Hillman [mailto:[log in to unmask]]

Sent: August-25-17 10:06 AM

To: TechNet E-Mail Forum <[log in to unmask]>; Steven Kelly <[log in to unmask]>

Subject: Re: [TN] Dried flux



Hi Steve - We use a number of "bga style" connectors where there is a solder charge/preform on the connector which is designed to combine with the solder paste deposit creating sufficient solder volume and good solder joint integrity. I am not familiar with the having these types of connectors with "dried flux" - flux has a shelf life so the manufacturer's comment doesn't make much sense. From a practical point, the flux in the solder paste deposit is doing the bulk of the oxide scrubbing action so dried flux contribution is most likely a moot point. But - the fact that the manufacturer did not acknowledge the possible shelf life issue is dis-concerning.



Dave Hillman

Rockwell Collins

[log in to unmask]<mailto:[log in to unmask]>



On Thu, Aug 24, 2017 at 1:11 PM, Steven Kelly <[log in to unmask]<mailto:[log in to unmask]>> wrote:

Hi All,

I have a new hi-density BGA connector I am trying to assemble. When the supplier makes the connector they "solder balls onto the pin" (lead free). We see dried flux on the balls and when we solder the connector we are getting a few joints with head in pillow. The connector manufacturer says the dried flux is not an issue - is this true? Thanks. Steve Kelly