In a message dated 4/10/2001 5:02:48 PM Central Daylight Time,
[log in to unmask] writes:
<< Steve/Shawn,
So how normally cured epoxy looks like? If you can post both, quick curing
v/s slow curing (regular) photos that will add more value to overall
discussion.
re,
ken patel >>
Hi Ken!
You bring up a good point, that'll be a project that shouldn't take too much
time that I'll tackle tomorrow...I'l try and post some pictures.
-Steve Gregory-
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|