TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wHElf-000BmXC; Tue, 15 Apr 97 15:23 CDT
Old-Return-Path:
Date:
Tue, 15 Apr 1997 16:13:53 -0500 (EST)
MIME-version:
1.0
Precedence:
list
Resent-From:
Cc:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11992
TO:
From [log in to unmask] Tue Apr 15 15:
40:13 1997
X-Loop:
Content-type:
TEXT/PLAIN; CHARSET=US-ASCII
Subject:
From:
Richard Krug <[log in to unmask]>
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"azFfk1.0.DQ8.FF-Kp"@ipc>
Message-id:
Resent-Sender:
TechNet-request [log in to unmask]
Parts/Attachments:
TEXT/PLAIN (22 lines)
We have occasionally seen problems during square wire pin insertion on PCB's 
which have been subjected to SMT reflow.  We use HASL PCB's.  We have measured 
diameters using pin gages.  Some times there is a measurable diameter change and
some times there is not.  I suspect the solder is melting in the barrel of the 
hole, but I would expect the soft solder to readily deform during the insertion 
process.  Any ideas of what could be happening?  

Dick Krug
[log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2