Hi,
We do reflow/cure,
One advantage is the positioning of board in stencil printing. Another is that
the soldering process is better controled than the gluing process so a glued
component may always fall down if the dot is too small or if the component is
hit.
Vincent Bada
Process Engineer
Alcatel ETCA
Charleroi
Belgium
-----
Not long ago, in Technet forum discussed running reflow/cure vs cure/reflow for
SMT double side assemblies. In my former life, I was happy running curing
bottom side first and reflowing top side later. Then wave solder bottom side.
I encountered no fuss, but it is a little bit of dilemma for now. Now, I am in
the middle of discussing a continuous SMT line for top and bottom side
assemblies. A few of companies that I visited in my former life run
"cure/reflow" process for continuous assembly lines, but one company I visited
recently run " reflow/cure" process.
Questions I want to throw at technet forum are;
What are your preferences?
What percentage of companies reflow/cure or cure/reflow processes?
What are pro's and con's of using either process for continuous assemblies?
telling you my preference is "cure/reflow" for continuous SMT assemblies. Main
reasons for my choice are: "can be easily changed to reflow/reflow", and " can
use a single cure profile" for many different products and a fast cool down
before processing top side assembly. One negative is positioning support pins
properly for top side printing.
Matthew S. Park
Sr. Process Engineer
Phoenix International Corp.
701-277-6434
[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|