This is one excellent reason that we allow NO separation in microsection
evaluations before or after Thermal Stress testing on the Lot conformance testing
prior to shipping you the boards to assemble.

If you had a test set and could actually operate the assemblies until they
"get hot" or experience a temperature rise, you might be able to pick up the
intermittencies.  These will then go away as the board cools down until you
finally exercise the inner layer connection to the point there is a hard open.

Susan Mansilla
Robisan Lab

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2