TECHNET Archives

September 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
R Sedlak <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Date:
Wed, 23 Sep 2009 10:25:18 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (55 lines)
Juan:  You may want to consider cleaning/deoxidizing existing silver, rather than re-plating.
Much easier/cheaper.

Rudy Sedlak
RD Chemical Company

--- On Wed, 9/23/09, Juan T. Marugán <[log in to unmask]> wrote:

From: Juan T. Marugán <[log in to unmask]>
Subject: [TN] IAg PCBs. Re-plating?
To: [log in to unmask]
Date: Wednesday, September 23, 2009, 9:06 AM

Hello,

I have a couple of questions for the PCBs specialist people.

We have a high quantity of boards plated with IAg. Most of them were 
manufactured before 2008. The questions are:

Is it possible to re-activate or re-plate the boards with the same finishing 
(IAg)? Risks?

Is it possible to remove the IAg and then to re-plate them with ENIG? Risks?

Thank you.

Juan T. Marugán
Indra Sistemas SA
Spain

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



      

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2