TECHNET Archives

August 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
David Girard <[log in to unmask]>
Reply To:
TechNet Mail Forum.
Date:
Thu, 7 Aug 1997 13:50:56 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (19 lines)
Bill,

I have no experience with customers taking exception to the J-STD but, I
have experienced many other customer exceptions to military
standards/specifications through the years.  Sometimes customers provide
their own workmanship standard or a tailored standard.  What does the
drawing call for on lead protrusion?  Typically drawing requirements
override "all" standards/specifications.  What type of equipment is this
to be used on?  Why do they want a solder joint with that much strength?