TECHNET Archives

November 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 11 Nov 2013 08:17:34 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Guy Ramsey <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
<01c701cedee0$62c5e4e0$2851aea0$@com>
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Guy Ramsey <[log in to unmask]>
Parts/Attachments:
text/plain (29 lines)
We have a customer in Korea using Samtec “Solder Charge” connectors.  The
alloy is SAC38 ( 95.5, 3.8, 0.7). 

They want to stay Pb-free.  

 

Our 60 layer, 480mm by  585 mm by  6.5 mm thick board, with  6100+ embedded
capacitors cannot survive the Z axis expansion seen at SAC reflow.  Test
samples have survived 10 reflows at 210°C.  

 

Has anyone tried to qualify the performance of SAC solder with SnBi solder
paste?  Does it have the same problems associated with mixing SAC and SnPb
paste? 

 

Thanks, 

Guy


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2