Hi Rex! Ah, it is good to be a material engineering these days as we don't
need to learn anything new, we just dig up old data sets! There have been
some good published work on tin pest in the last couple of years. In fact,
Dr. Chris Hunt of the NPL has done some of the newest cutting edge work. I
recommend you go to the NPL's website and download his reports on tin
pest. Rockwell Collins also has published some investigation results which
I'll send to you. The current industry "thoughts" on tin pest is that
leadfree electronics are at low risk of the phenomena causing issues.
Dave Hillman
Rockwell Collins
[log in to unmask]
Rex Waygood <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
12/22/2008 09:14 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Rex Waygood <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Tin Pest
Can someone tell me why I should not worry?
I am told that tin pest has not occurred in electronic circuits where
lead free (high tin) alloys have been used for years.
I have seen the NPL video where tin pest propagates rapidly from a
seeded tin bar into lead free alloys that were anticipated to be immune.
When I buy components now it is likely they have a matt tin plating.
(Probably not the case historically)
Is that plating likely to be a seed for a lead free solder joint?
I have customers where the end product goes to some very cold places,
they are not RoHS exempt, so what do I advise them?
Rex Waygood
Technical Manager
PartnerTech Poole Ltd
Benson Road
Poole
Dorset BH17 0RY
United Kingdom
Tel: +44 (0)1202 674333
Fax: +44 (0)1202 678028
DDI: +44 (0)1202 338222
Mob: +44 (0)7887 997403
[log in to unmask]
www.PartnerTech.co.uk
-------------------------------------------------------------------------------
The information contained within this e-mail and any attachments contained
therein may be confidential and/or legally privileged and is for the use
of the intended recipient only. If you are not the intended recipient
please delete it from your system and notify the sender by return e-mail.
The content of this e-mail may not be copied or disclosed to any third
parties without prior permission from the sender.
E-mail is susceptible to data corruption, interception, tampering and
viruses. We do not accept any liability for any such incidents or any
consequences thereof.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|