Howard:
I can't help asking: why do you remove no clean flux residues?
Jim Smith
Managing Director
Electronics Manufacturing Sciences, Inc.
4285 45th St. S.
St. Petersburg, FL 33711-4431
Tel: (727)866-6502 ext. 21
Fax: (727)867-7890
eMail: [log in to unmask]
Howard Watson wrote:
>
> Jim,
>
> Interesting that you ask, as I was just in the process of ordering
> some more of the pens that we use, which is called a "Pad Prep Pen",
> made by A.P.E. , P/N is 8200-1350, 8 for $89. I don't have experience
> with any others, so I won't place judgement. However, our operators
> love this one for removing our no-clean flux residue.
>
> Howard Watson
> SMT Manufacturing Engineer
> AMETEK/Dixson
>
>
>
> "West, Jim" <[log in to unmask]>
> Sent by: TechNet <[log in to unmask]>
>
> 07/09/03 01:41 PM
> Please respond to "TechNet E-Mail Forum."; Please respond to "West, Jim"
>
>
> To: [log in to unmask]
> cc:
> Subject: [TN] No clean flux remover pen
>
>
>
>
> Good afternoon,
>
> I was informed by my purchasing department that Multicore (part #
> MC-PV-01) is no longer making their Mini-cleaner (prozone pen), that
> we were using to remove flux residue from hand soldered applications.
> We have received a sample from a different supplier that is supposed
> to do the same thing, the only problem is the pen leaks severely when
> you push on the tip. This may be a bad sample, but we are not off to
> a good start trying to find a replacement. Does anyone else out there
> use these types of pens to remove flux residue from hand soldering or
> similar applications? If so, what manufacturer do you use and how do
> the pens perform? You can email me off-line if you like.
>
> Thanks,
> Jim West
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
> in the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
> in the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|