In addition to what Graham has said about salts under conformal coating,
consider also that when a salt crystal encounters water, which WILL come
through conformal coatings, it will expand up to 200 times its original
volume, creating a localized blister.  This effect is often referred to as
"mealing".  Once the blister is formed, it is a place for water vapor to
collect and condense.  Liquid water together with the original salt material
forms an electrolytic solution, which is generally detrimental to circuit
reliability.

Doug Pauls
CSL

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2