Phil,
Most of the pure acrylic coatings are not that good in terms of chemical
resistance. We do not allow our conformally coated assemblies (Humiseal
1B31) to go through saponified aqueous cleaning for just the reason you
are seeing, the adhesion gets affected and the coating comes off.
Doug Pauls
Phil Nutting <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
05/27/2008 07:46 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Phil Nutting <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Conformal coating washing off
Brian,
I guess I should add that we have been using this conformal coating for
about six years with "great success". It has only been in this test of a
new washing system that we are seeing the coating peel off. The DI wash
in my original post was the wash step after soldering with an OA flux.
Maybe the detergent in the wash system is really good for cleaning
conformal coating off the boards... if that was what I really wanted.
Phil
-----Original Message-----
From: Brian Ellis [mailto:[log in to unmask]]
Sent: Saturday, May 24, 2008 2:04 AM
To: TechNet E-Mail Forum; Phil Nutting
Subject: Re: [TN] Conformal coating washing off
Some types of solder mask contain nasties that may prevent a decent
adhesion of a CC or they may not have been properly polymerised, leaving
insoluble monomers or other components on the surface. I suggest you
start looking in this direction.
Brian
Phil Nutting wrote:
> We are using Chemtronics Konform AR on some circuit boards. The boards
are batch washed in DI water and pre-baked prior to coating and then cured
in a 60° or 77° C oven.
>
> In a recent test of a new washing system where we are removing slip ring
dust (brass and carbon) on these boards and dielectric oil from other
boards and aluminum castings, I noticed the conformal coating peeling off
in sheets after both the wash and DI rinse cycles. Both wash and rinse
are between 140 and 150° F.
>
> Is this stuff peeling off because of the water temperature, poor
pre-coating prep or possibly something else?
>
> Thanks in advance,
>
> Phil
>
> Note: All the information contained in this e-mail and its attachments
is proprietary to Kaiser Systems, Inc. and it may not be reproduced
without the prior written permission of sender. If you have received this
email in error, please immediately return it to sender and delete the copy
you received.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
> -----------------------------------------------------
>
Note: All the information contained in this e-mail and its attachments is
proprietary to Kaiser Systems, Inc. and it may not be reproduced without
the prior written permission of sender. If you have received this email
in error, please immediately return it to sender and delete the copy you
received.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|