TECHNET Archives

June 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
"Thorup, John" <[log in to unmask]>
Date:
Thu, 3 Jun 1999 13:04:20 -0700
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum.\" <[log in to unmask]>, \"Thorup, John" <[log in to unmask]>
Parts/Attachments:
text/plain (64 lines)
I think I've seen every type of polar component mis-marked of the years
- keeps you on your toes.  Seems to me I remember something  about the
smoke from fried tantalums being toxic so it might be prudent to add
ventilation to the safety precautions.

>-----Original Message-----
>From:  Raymond Klein [SMTP:[log in to unmask]]
>Sent:  Thursday, June 03, 1999 12:45 PM
>To:    [log in to unmask]
>Subject:       Re: [TN] Tantalum caps and the big bang
>
>Ron,
>
>In the past 20 or so years I've seen about 6 lots of tant caps the were
>polarity mis-labeled. They get quite hot and pop. One even smoked a trace
>on the PWB. (My fault for making it too thin).
>
>You can test caps by putting them directly across a DC supply at 1/2 the
>rated voltage. The supply should be able to supply at least 1 amp. If the
>cap gets hot in a few seconds its "+" lead (what ever its marking) is
>connected to the "-" lead of the power supply. Wear safety goggles as com
>caps can fail spectacularly. Also be careful touching them as they can
>raise a blister.
>
>Good luck - Ray Klein
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
>for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>847-509-9700 ext.312
>################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2