Rick Pfeiffer <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 27 Oct 2006 09:59:09 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (130 lines)
Steve,

I think I saw your picture on the side of the mountain.

Rick Pfeiffer
330-796-5904
[log in to unmask]


                                                                           
             Steve Gregory                                                 
             <SGregory@OAIELEC                                             
             TRONICS.COM>                                               To 
             Sent by: TechNet          [log in to unmask]                     
             <[log in to unmask]>                                          cc 
                                                                           
                                                                   Subject 
             10/27/2006 08:13          [TN] NTC - Friday's Enigma...       
             AM                                                            
                                                                           
                                                                           
             Please respond to                                             
              TechNet E-Mail                                               
                   Forum                                                   
             <[log in to unmask]>                                             
             ; Please respond                                              
                    to                                                     
               Steve Gregory                                               
             <SGregory@OAIELEC                                             
               TRONICS.COM>                                                
                                                                           
                                                                           




Good Morning All!

YAY! It's Friday!! Today's Friday Enigma will be a test of your powers
of observation.

There are two pictures identical to each other.  You have to find three
differences between the two.

If you can find three differences, then you are a part of an elite group
of individuals.

This has been tested on many people, and hardly anyone found the three
differences.

I can only manage to find two. Let me know if you find all three.

The third must be impossible to find!  Click on the link below to see
the two pictures:

http://members.home.nl/saen/Special/Zoeken.swf
<http://members.home.nl/saen/Special/Zoeken.swf>


-Steve Gregory-


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


***************************************************************************
CONFIDENTIALITY  NOTICE: The materials attached hereto are confidential and
the property of the  sender. The information contained in the attached
materials is privileged and/or confidential and  is  intended only for the
use of the above-named individual(s) or entity(ies). If  you are not the
intended recipient, be advised that any unauthorized disclosure,  copying,
distribution or the taking of any action in reliance on the contents of
the attached information is strictly prohibited. If you have received this
transmission in error, please discard the information immediately.


ITAR NOTICE: This email may contain technical data which may be controlled
by the US International Traffic and Arms Regulation (ITAR) 22 CFR part
120-130.  If this data is determined to be ITAR controlled, such data may
not be transmitted, shared or provided to any foreign party or entity
either
verbally or visually with out proper licenses from State Department. It is
your responsibility to assure this item can be legally shared with another
party.  See ABSC's Export Compliance Officer if you have any questions
regarding this requirement.
***************************************************************************

***************************************************************************
CONFIDENTIALITY  NOTICE: The materials attached hereto are confidential and
the property of the  sender. The information contained in the attached
materials is privileged and/or confidential and  is  intended only for the
use of the above-named individual(s) or entity(ies). If  you are not the
intended recipient, be advised that any unauthorized disclosure,  copying,
distribution or the taking of any action in reliance on the contents of
the attached information is strictly prohibited. If you have received this
transmission in error, please discard the information immediately.


ITAR NOTICE: This email may contain technical data which may be controlled
by the US International Traffic in Arms Regulation (ITAR) 22 CFR part
120-130.  If this data is determined to be ITAR controlled, such data may
not be transmitted, shared or provided to any foreign party or entity either
verbally or visually without proper licenses from the State Department. It is
your responsibility to assure this item can be legally shared with another
party.  See ABSC's Export Compliance Officer if you have any questions
regarding this requirement.
***************************************************************************

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2