Nitric is very aggressive. I wouldn't use it for cleaning copper oxide. You
risk inducing a grainy copper  surface, pitting, etc. etc.

A 10% sulfuric solution has worked great for me for years.

Hope this helps

Franklin D Asbell

-----Original Message-----
From: nishath yasmeen <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Friday, July 23, 1999 2:40 PM
Subject: [TN] Copper oxide removal


>Hello everyone!
>    Is Nitirc acid ( dilute)  a better acid than sulfuric for cleaning
>the oxide on plated copper?
>    Any information provided will be appreciated.
>
>Yasmeen
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2