750°F is about right for good ol' through hole parts, light connectors that
you might be "touching up" at the end of a wave solder step. It could be too
high for sensitive components, micro-connectors, SMT passives, and the like.

What is the shape of the tip? Rate of heat transfer is the real issue. If
you have a quarter inch chisel tip at 750° it's probably too much. A conical
tip at that temperature might be appropriate for general purpose use. A
skilled operator will take advantage of the tip shape to control heat
transfer.

Guy Ramsey
American Competitiveness Institute
Senior Lab Technician / Instructor
610 362-1200 ext. 107


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Becerra Alejandro
Sent: Wednesday, February 21, 2001 6:11 PM
To: [log in to unmask]
Subject: [TN] Temperatures for Rework operation


Hello to All,

I am interested in the optimum temperature for the soldering iron used in
rework operations.
At this moment we use 750F (Aprox. 400C) in the soldering irons for the
touch up operation (Rework operation in line for wave soldering).
Is it correct this temperature or do we use a lower temperature?

Thanks in advance



Alejandro Becerra
Quality Assurance
Phone (915) 841-8439, Fax (915) 841-8401
[log in to unmask]

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2