IPC sells training kits, all kinds of them depending on what you are trying to train. They have training boards with BGAs, with SOICs, with bottom terminated components (QFNs, etc). You can also buy them from Practical Components http://practicalcomponents.com/
Or Topline Components http://www.topline.tv/Kits.html
Or Heraeus.
We use these to train our operators first to assemble (hand assembly and machine assembly) but we make sure they create a few defects purposely, then the same boards and parts can be used to train and certify rework operators and inspectors.
I don't recommend ever attempting to use old scrap electronics for solder training, as the components may be so oxidized they will no longer solder.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: Monday, July 23, 2012 1:01 PM
To: [log in to unmask]
Subject: Re: [TN] IPC J-STD-001 Boards for the inspection lab of training
Katy,
The best is go to some local electronic active surplus store and buy few of boards (they might be mount on old computer chassis, or system etc). I used to go to one of the surplus store and look at the "X" board and try to figure out why it is not working. You learn a lot look at different layout and mounting without have to deal with NDAs or other problems (except the nasty look of the store owner if you don't buy something - I usually do buy some junk for prototype, copper sheet, fan, etc).
Joyce Koo
Materials Researcher - Materials Interconnect Lab Research In Motion Limited
Office: (519) 888-7465 79945
Mobile: (226) 220-4760
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ballas, Katy
Sent: Monday, July 23, 2012 1:43 PM
To: [log in to unmask]
Subject: [TN] IPC J-STD-001 Boards for the inspection lab of training
Hello fellow technetters!
I have an issue that I hope someone can help me with. I need to get my hands on some PCB boards to use in the inspection lab for 001 training. The issue that I have is that I do not work in a board shop, where I work we solder cables and due to this we need to have some people trained to J-STD-001E. Does anyone out there have a couple populated boards that either have defects (or I can create them) they would be willing to give me? Otherwise, are there sources out there that sell populated boards for this purpose? Thanks in advance.
Katy Ballas
Manufacturing Process Engineer
Molex Incorporated
[cid:[log in to unmask]]
________________________________
CONFIDENTIALITY NOTICE: This message (including any attachments) may contain Molex confidential information, protected by law. If this message is confidential, forwarding it to individuals, other than those with a need to know, without the permission of the sender, is prohibited.
This message is also intended for a specific individual. If you are not the intended recipient, you should delete this message and are hereby notified that any disclosure, copying, or distribution of this message or taking of any action based upon it, is strictly prohibited.
English | Chinese | Japanese
www.molex.com/confidentiality.html
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|