Hi Kenny - one more bit of information you may want to take a look at -
"Connector Contacts: Critical Surfaces", author Robert Mroczkowski of AMP
Inc, Advanced Materials & Processes inc. Metal Progress, 12/88, pages
49-52. This reference covers the basics very well and talks about the
pros/cons of tin. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Kenny Bloomquist <[log in to unmask]> on 12/02/98 10:29:34 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Kenny Bloomquist <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Gold and Tin Interconnect
We have an assembly that uses tin plated pins and sockets for the
interconnection. We are having trouble getting the pin side in tin but is
readily available in gold. My question is "is there any long term problems
putting a gold pin in a tin plated socket"?
For years people have put I/C leads into gold sockets without problem so it
seems that this should not be a problem but thought I'd ask for any real
life experiences.
Thanks,
Ken Bloomquist
Sr. Principal Process Engineer
PRIMEX Aerospace Company
P.O. Box 97009
Redmond, WA 98073-9709
www.primextech.com
Ph: 425-885-5000
FAX: 425-882-5786
[log in to unmask]
Northcon/98, Show Director
<www.northcon.org>
Electronics Manufacturers Association (EMA), Secretary
<www.ema-wa.org>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|