Hi Kenny - one more bit of information you may want to take a look at - "Connector Contacts: Critical Surfaces", author Robert Mroczkowski of AMP Inc, Advanced Materials & Processes inc. Metal Progress, 12/88, pages 49-52. This reference covers the basics very well and talks about the pros/cons of tin. Good Luck. Dave Hillman Rockwell Collins [log in to unmask] Kenny Bloomquist <[log in to unmask]> on 12/02/98 10:29:34 AM Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to Kenny Bloomquist <[log in to unmask]> To: [log in to unmask] cc: Subject: [TN] Gold and Tin Interconnect We have an assembly that uses tin plated pins and sockets for the interconnection. We are having trouble getting the pin side in tin but is readily available in gold. My question is "is there any long term problems putting a gold pin in a tin plated socket"? For years people have put I/C leads into gold sockets without problem so it seems that this should not be a problem but thought I'd ask for any real life experiences. Thanks, Ken Bloomquist Sr. Principal Process Engineer PRIMEX Aerospace Company P.O. Box 97009 Redmond, WA 98073-9709 www.primextech.com Ph: 425-885-5000 FAX: 425-882-5786 [log in to unmask] Northcon/98, Show Director <www.northcon.org> Electronics Manufacturers Association (EMA), Secretary <www.ema-wa.org> ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################