Was finally able to sacrifice a board for cross section and sem and we ran a lot of bare boards through reflow.
It seems the spots are indeed solder. Thanks for all of the input.
Confidentiality Notice: The information contained in this message is intended only for the use of the addressee, and may be confidential and/or privileged. If the reader of this message is not the intended recipient, or the employee or agent responsible to deliver it to the intended recipient, you are hereby notified that any dissemination, distribution of copying of this communication is strictly prohibited. if you have received this communication in error, please notify the sender immediately.
Warning: This document may contain technical data within the definition of the International Traffic in Arms Regulation (ITAR) and is subject to the export control laws of the U.S. Government. Transfer of this data by any means to a foreign person, whether in the United States or abroad, without an export license or other approval from the U.S. Department of State, is strictly prohibited
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Wednesday, July 30, 2014 8:05 AM
To: [log in to unmask]
Subject: Re: [TN] Spots on Gold
Just a little history
We tend to build very small lots.
So this run was 6 pieces of 2 different boards.
Out of the 12 total pieces we had these spots on 8 boards.
All of the boards came out of the same FAB shop. I know this FAB shop outsources Their ENIG.
All of the spots have this black ring like someone took a magic marker and circled them.
Going to get on the SEM today and I am trying to find a XRF we can use. But more runs At the assembly shop and cross sections are probably next.
Confidentiality Notice: The information contained in this message is intended only for the use of the addressee, and may be confidential and/or privileged. If the reader of this message is not the intended recipient, or the employee or agent responsible to deliver it to the intended recipient, you are hereby notified that any dissemination, distribution of copying of this communication is strictly prohibited. if you have received this communication in error, please notify the sender immediately.
Warning: This document may contain technical data within the definition of the International Traffic in Arms Regulation (ITAR) and is subject to the export control laws of the U.S. Government. Transfer of this data by any means to a foreign person, whether in the United States or abroad, without an export license or other approval from the U.S. Department of State, is strictly prohibited
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Wednesday, July 30, 2014 7:55 AM
To: [log in to unmask]
Subject: Re: [TN] Spots on Gold
This is starting to get very interesting and worrisome.
That is indeed a linear tech umodule. We do pre-bump the devices before the install.
I found out last night we actually have a SEM, even though we have L3 in the name we are a very small division. But I am going to work through all of the suggestions until we get to the bottom of it. If this is indeed a plating issue that would be really really really Bad.
Once again I really appreciate all of the input.
John
Confidentiality Notice: The information contained in this message is intended only for the use of the addressee, and may be confidential and/or privileged. If the reader of this message is not the intended recipient, or the employee or agent responsible to deliver it to the intended recipient, you are hereby notified that any dissemination, distribution of copying of this communication is strictly prohibited. if you have received this communication in error, please notify the sender immediately.
Warning: This document may contain technical data within the definition of the International Traffic in Arms Regulation (ITAR) and is subject to the export control laws of the U.S. Government. Transfer of this data by any means to a foreign person, whether in the United States or abroad, without an export license or other approval from the U.S. Department of State, is strictly prohibited
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Wednesday, July 30, 2014 5:02 AM
To: [log in to unmask]
Subject: [TN] Spots on Gold
Morning John,
I have your second photo posted, it's here:
http://stevezeva.homestead.com/ring.jpg
This looks interesting!
Steve
On Tue, Jul 29, 2014 at 5:56 PM, <[log in to unmask]> wrote:
> Hi steve
>
> I managed to get to a good microscope this afternoon. Everyone of
> these spots looks like someone circled it* w*ith a magic marker.
>
> Would you mind posting one more pic for me.
>
> Thanks
>
> John Foster
>
>
>
--
This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|