TECHNET Archives

June 2011

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Gregg Owens <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Gregg Owens <[log in to unmask]>
Date:
Wed, 1 Jun 2011 14:20:19 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (106 lines)
Doug:

Does this mean we are all really blind but just quantitatively don't know it?

Gregg Owens 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Wednesday, June 01, 2011 2:20 PM
To: [log in to unmask]
Subject: Re: [TN] Should inspectors be able to see?

Don,
This topic has come up from time to time in the J-STD-001 and IPC-A-610 
committee meetings.  Vision is usually assumed to be corrected to 20/20 
and you go from there.  Several individuals in the committees, who deal 
more with oversees usage of A-610 indicate that "20/20" or "3 diopters", 
are American terms and have no meaning oversees.  I confirmed that with my 
brother-in-law, a doctor of optometry, who confirmed that there is no 
international standard for visual acuity. 

Doug Pauls



Don McFarland <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
06/01/2011 01:25 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Don McFarland <[log in to unmask]>


To
<[log in to unmask]>
cc

Subject
[TN] Should inspectors be able to see?






Does anyone have a standard for an inspector's ability to see? We have 
required them to pass color-blind testing in the past, but have recently 
mulled over a visual acuity requirement. I wondered if this is more normal 
than not, because it seems like we would want to ensure that they see 
lines with definition rather than blurry masses. 

I humbly look forward to any input that may be offered. 

Don

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2